Strontium modification is essential in the production of structurally
sound and dimensionally accurate Al-Si castings and fabricated
products. Strontium offers clear advantage over sodium or antimony-based
alloy additives, including safer addition, better recovery,
reduced fade and a
fume-free application.
|
 |
| |
¢º Reduced tendency for hot-tearing
¢º Improved mechanical properties
¢º Reduced evenly distributed porosity
¢º Enhanced compositional homogeneity
¢º Better response to heat treatment
¢º Improved surface finish
|
 |
| |
* Different composition(%) of alloys available upon
customer¡¯s request.
(Please click composition for the further information)
Element |
Composition(%) |
Color Code |
Aluminum Strontium
|
AlSr5% |
Light
blue |
|
AlSr10% |
Light
blue |
|
AlSr15% |
Light
blue
|
|
 |
| |
|
SLM
|
Competitor
|
Type |
Rod, Plate, Bar type |
Waffle |
|
18kg/mm2 |
16kg/mm2
|
|
10%
|
7% |
Recovery
|
More than 97% |
80-85% |
Porosity
|
Less
|
more |
| Particle Size |
minute
|
Not minute |
Particle distribution
|
uniform
|
Not uniform |
| Diffusion Velocity |
high
|
low |
Diffusion Time
|
Less than 10 min |
More than 30 min |
Product Size
|
customized
|
Specific cutting |
|
|
|